Inconel X750 Pipe Features
- Non-magnetic
- Excellent fatigue resistance
- Ease of fabrication
- High strength pipes
- 80-90% Anti-corrosion
Inconel X750 Pipe
Inconel X750 pipes refers to pipes made from nickel-chromium-based alloy. It exhibits high tensile strength and resistance to cracking in harsh environments. They can withstand well in extreme temperatures, up to 1300°F (704°C) without undergoing deformation.
Pipes made from Inconel X750 are used as aircraft engine components and gas turbine parts in aerospace industry. In the oil and gas industry, they are used as downhole tools, wellhead components, and tubing hangers. Lastly, Inconel X750 pipes are used as seawater desalination plants and offshore platforms in marine industry.
If you choose Tuolian, we can customize Inconel X750 pipes into your preferred sizes, surface finishes, and end connections. This allows you to get the specific pipes for your particular application.
For your concerns about our services and Inconel X750 pipes, please contact us.
- Main Types
- Pipe Measurements
- Mechanical Properties
- Chemical Composition
Seamless Types
Seamless pipes are made from a single piece of Inconel X750 material. And it does not have any welded joints or seams. They are preferred in where a high level of corrosion resistance is required, as they have fewer potential leak points.
Welded Types
Welded Inconel X750 Pipe is made by welding multiple pieces of Inconel X750 material together. They are preferred in where larger pipe sizes are required, as they can be manufactured in larger diameters than seamless pipes.
Nominal Pipe Size | Outside Diameter | Wall Thickness (per inches) | Length (per ft) |
1/8″ | 0.405″ | 0.068″ | 10 |
1/4″ | 0.540″ | 0.088″ | 10, 20 |
3/8″ | 0.675″ | 0.091″ | 10, 20 |
1/2″ | 0.840″ | 0.109″ | 10, 20 |
3/4″ | 1.050″ | 0.113″ | 10, 20 |
1″ | 1.315″ | 0.133″ | 10, 20 |
2″ | 2.375″ | 0.154″ | 10, 20 |
3″ | 3.500″ | 0.216″ | 10, 20 |
5″ | 5.563″ | 0.258″ | 10, 20 |
10″ | 10.750″ | 0.365″ | 10, 20 |
Yield Strength | 70 ksi |
Elongation | 25% minimum |
Hardness | Rockwell C 35 maximum |
Modulus of Elasticity | 31.0 x 10^6 psi |
Poisson’s Ratio | 0.32 |
Density | 8.28 g/cm^3 |
Melting Point | 1,290 °C |
Thermal Expansion Coeff | 14.0 x 10^-6 m/m/°C |
Thermal Conductivity | 12.1 W/m-K |
(Ni) | 70.0% – 75.0% |
(Cr) | 14.0% – 17.0% |
(Fe) | 5.0% – 9.0% |
(Co) | 1.0% – 2.5% |
(Mn) | 1.0% max |
(Cu) | 0.5% max |
(Al) | 0.4% – 1.0% |
(Ti) | 2.25% – 2.75% |
(Si) | 0.5% max |
(C) | 0.08% max |
(S) | 0.01% max |
(P) | 0.01% max |