X6CrNiTi18-10 Stainless Steel
- Excellent toughness
- High-temperature strength
- Low thermal expansion
- High oxidation resistance
- Good scaling resistance
- Low magnetic permeability
- Resistant to stress corrosion cracking
- Uniform corrosion resistance
- Resistant to pitting and crevice corrosion
- Easy to clean and maintain
X6CrNiTi18-10 Stainless Steel Manufacturer
X6CrNiTi18-10 stainless steel is a type of austenitic stainless steel. It contains chromium, nickel, and titanium element. The addition of titanium also enhances its resistance to intergranular corrosion.
This austenitic stainless steel is a widely used material in various industrial applications due to its exceptional corrosion resistance, high strength, & excellent formability. It also withstands heavy loads and high temperatures without losing its structural integrity.
The chemical composition of X6CrNiTi18-10 stainless steel is strictly regulated by international standards. Thus, ensuring consistent quality and performance. It is accessible in a broad array of shapes and sizes, including bars, tubes, sheets, and plates, to meet different application requirements.
For your unique requirements, Tuolian provides a highly customized service. This allows for meeting customer specifications quickly & easily. Message us for more details!
Extensive Applications
- Food processing equipment
- Pressure vessels and tanks
- Chemical processing industry
- Heat exchangers
- Domestic kitchenware
- Automotive
- Architectural
- Marine applications
- Fasteners and springs
- Petrochemical
- Aerospace component
- Pharmaceutical industry

- Mechanical Properties
- Chemical Composition
- Standard
Parameters | Specifications |
Grade designation | X6CrNiTi18-10 |
Steel Type | Austenitic stainless steel |
Density | 7.9 g/cm³ |
Melting Point | 1400-1450 °C |
Tensile Strength | 500-700 MPa |
Yield Strength | 200-250 MPa |
Modulus of Elasticity | 190-210 GPa |
Elongation at Break | 40-50% |
Hardness, Rockwell B | 80 |
Impact Strength | 100-150 J |
Poisson’s Ratio | 0.3 |
Thermal Conductivity | 15-25 W/m.K |
Specific Heat Capacity | 500 J/kg.K |
Electrical Resistivity | 0.75 x 10^-6 Ω.m |
Element | Composition (%) |
Carbon | ≤ 0.08 |
Silicon | ≤ 1.00 |
Manganese | ≤ 2.00 |
Phosphorus | ≤ 0.045 |
Sulfur | ≤ 0.030 |
Chromium | 17.0 – 19.5 |
Nickel | 10.0 – 12.0 |
Titanium | 5 x C – 0.7 or ≤ 0.80 |
Iron | Balance |
Standard | Purpose |
EN 10088-1 | Defines the technical delivery conditions for hot or cold rolled sheets/plates, strips, and bars for general purposes. |
EN 10216-5 | Specifies the technical delivery conditions for seamless steel tubes for pressure purposes. |
EN 10217-7 | Specifies the technical delivery conditions for welded steel tubes for pressure purposes. |
ASTM A312/A213/A269 | Specifies the technical requirements for seamless and welded austenitic stainless steel pipes. |
ASTM A240/A480 | Specifies the technical requirements for general-purpose and heat-resisting chromium and chromium-nickel stainless steel plate, sheet, and strip. |
ASTM A276/A479 | Specifies the technical requirements for hot or cold finished bars and shapes made from stainless steel. |